Alloy elements in steels have influence on the welding

Editor:    Date:2014-07-30 17:23:47    Views:6666

Alloy elements in steels have influence on the welding
Aluminum: aluminum is used as a cleaning agent grain refinement and deoxidization. Aluminum can significantly reduce the strain aging brittleness, excess aluminum will reduce the toughness of steels.
S: for the harmful elements, which makes the plasticity and toughness of steel decreases, especially the toughness effect is more apparent, have an adverse effect on the welding.
P: harmful elements, slashing the plasticity and impact toughness, improve the brittle temperature of steel, steel welding crack susceptibility.
The above is the alloy elements in Shenzhen sushi heat treatment summary of the impact of welding, Shenzhen Su's heat treatment to undertake professional stainless steel welding, aluminum brazing, heat treatment orders.

Prev: Shenzhen Su's heat treatment and compound modification processing of Zr and Ti on the microstructure of ZA27 alloy obtained three conclusions Next: Alloy steel heat treatment process of the role
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance corrosion and wear resistance
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance to corrosion and wear properties of a great relationship: the number and morphology of precipitates in the pure wear conditions, no corrosion, material quality loss is influenced by mechanical factors.
Vacuum heat treatment of the problem
Vacuum heat treatment processing, the processing surface of the product is often a problem, "colored" areas appear. Obtain appearance of bright, no coloring effect is the common goal of product processing vacuum furnace manufacturers and users to pursue research and development.
Vacuum heat treatment technology to resolve
Comprehensive technology of vacuum heat treatment vacuum technology and heat treatment technology of two professional combination, refers to the heat treatment process of all or part of the vacuum condition. Is generally believed that the vacuum furnace is divided into high, high, medium and low vacuum.
Factors that affect the performance of the heat treatment
Today su shi heat treatment come to you of what the factors in the use of vacuum heat treatment furnace heat treatment will affect the performance of the heat treatment:

1
Brazing of aluminum frame
Product:Brazing of aluminum frame
2Cold die steel heat treatment technology
3High-frequency quenching
4Stainless solution treatment
5SUS420 blade heat treatment
6Vacuum hardening

Similar Articles

Latest News

History

Set Home Page  |Contact|News|Set Map

Su's heat treatment (Shenzhen) Co., Ltd.  Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14

(Workdays:9:30-18:00)

Online QQ



Service Hotline

0755-27291255