Alloy steel heat treatment process of the role:
C: plays an important role on the strength of steel, but the carbon content should not be too high or too low, too high will affect the welding performance and increased brittleness, low strength of steel would be decreased.
Manganese: strongly increase the hardenability of steel, has little effect on the stability of tempering. Nickel: increase the toughness of the steel, and can improve the impact resistance of low temperature gap, have good fatigue resistance.
To improve the effect of quenching and tempering stability. Mo: to improve the hardenability and tempering stability have significant effects.
Mo: to improve the hardenability and tempering stability have significant effects.
Cr: significantly improve the hardenability of the steel and enhance the stability of the temper, to improve the wear resistance of steel and steel oxidation, corrosion resistance. Chromium is promoting the temper brittleness of elements, in the given conditions of temper brittleness with increasing chromium content and more pronounced.
Shenzhen Su's heat treatment has been trying to study, improve heat treatment process!

Prev: Shenzhen Su's heat treatment to undertake professional stainless steel welding, aluminum welding Next: Shenzhen Su's heat treatment of 40Cr steel gear surface punctate stripping failure analysis, draws the conclusion and suggestions to share with you:
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance corrosion and wear resistance
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance to corrosion and wear properties of a great relationship: the number and morphology of precipitates in the pure wear conditions, no corrosion, material quality loss is influenced by mechanical factors.
Vacuum heat treatment of the problem
Vacuum heat treatment processing, the processing surface of the product is often a problem, "colored" areas appear. Obtain appearance of bright, no coloring effect is the common goal of product processing vacuum furnace manufacturers and users to pursue research and development.
Vacuum heat treatment technology to resolve
Comprehensive technology of vacuum heat treatment vacuum technology and heat treatment technology of two professional combination, refers to the heat treatment process of all or part of the vacuum condition. Is generally believed that the vacuum furnace is divided into high, high, medium and low vacuum.
Factors that affect the performance of the heat treatment
Today su shi heat treatment come to you of what the factors in the use of vacuum heat treatment furnace heat treatment will affect the performance of the heat treatment:

1
Brazing of aluminum frame
Product:Brazing of aluminum frame
2Cold die steel heat treatment technology
3High-frequency quenching
4Stainless solution treatment
5SUS420 blade heat treatment
6Vacuum hardening

Similar Articles

Latest News

History

  • None
Set Home Page  |Contact|News|Set Map

Su's heat treatment (Shenzhen) Co., Ltd.  Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14

(Workdays:9:30-18:00)

Online QQ



Service Hotline

0755-27291255