40Cr Quench

Editor:    Date:2014-04-10 11:27:52    Views:8056

The quenching process of 40 cr

40 to 850 ℃, cr quenching oil cooling; Around 520 ℃ tempering, soon cold.


Surface quenching hardness of HRC52-60, flame quenching can achieve HRC48-55.

40 cr nitriding processing

40 cr are nitrided steel, its elements for nitriding. 40 cr after nitriding treatment can obtain higher surface hardness, 40 cr after quenched and tempered nitriding processing hardness can top HRA72 ~ 78, namely HRC43 ~ 55.

N chemical process routes: forging, annealing - rough machining - conditioning - finishing - in addition to the stress and coarse grinding - nitride - fine grinding and grinding. Because nitride thin and brittle, and therefore requires a higher intensity is the heart of the organization, so need to tempering heat treatment, get tempered sorbite, mechanical properties and nitride layer quality of improving the core. Soft nitriding is reactive nitrogen, is now more commonly used gas nitriding.

Prev: DC53 heat treatment Next: S136 heat treatment
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance corrosion and wear resistance
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance to corrosion and wear properties of a great relationship: the number and morphology of precipitates in the pure wear conditions, no corrosion, material quality loss is influenced by mechanical factors.
Vacuum heat treatment of the problem
Vacuum heat treatment processing, the processing surface of the product is often a problem, "colored" areas appear. Obtain appearance of bright, no coloring effect is the common goal of product processing vacuum furnace manufacturers and users to pursue research and development.
Vacuum heat treatment technology to resolve
Comprehensive technology of vacuum heat treatment vacuum technology and heat treatment technology of two professional combination, refers to the heat treatment process of all or part of the vacuum condition. Is generally believed that the vacuum furnace is divided into high, high, medium and low vacuum.
Factors that affect the performance of the heat treatment
Today su shi heat treatment come to you of what the factors in the use of vacuum heat treatment furnace heat treatment will affect the performance of the heat treatment:

1
Brazing of aluminum frame
Product:Brazing of aluminum frame
2Cold die steel heat treatment technology
3High-frequency quenching
4Stainless solution treatment
5SUS420 blade heat treatment
6Vacuum hardening

Similar Articles

Latest News

History

Set Home Page  |Contact|News|Set Map

Su's heat treatment (Shenzhen) Co., Ltd.  Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14

(Workdays:9:30-18:00)

Online QQ



Service Hotline

0755-27291255