Client
ASP-23 CPM

Editor:    Date:2014-04-10 11:25:50    Views:8589


Introduction: ASP23 is steel, chrome vanadium molybdenum powder belongs to the Swedish standard, a Swedish wins the typical representative, with series of ASP - 30, ASP - 60 powder high speed steel.


Product features: high wear resistance, high strength, good toughness, good heat treatment of dimensional stability, good temper softening resistance and very good hardenability factory status: HB 260 or higher


Surface treatment: the high alloy tool steel processing and heat treatment, are usually more difficult than low alloy tool steel, so the mould manufacturing costs are high, and powder metallurgy manufacturing ASP - 23, its machinability, than the conventional method of manufacturing high alloy tool steels is also good, the size stability of the heat treatment is also good, and easy to predict. More because of its high hardness, high toughness and high temperature tempering features, especially suitable for surface treatment, such as PVD titanium coating.

Prev: Bright annealed stainless steel 304 Next: DC53 heat treatment
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance corrosion and wear resistance
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance to corrosion and wear properties of a great relationship: the number and morphology of precipitates in the pure wear conditions, no corrosion, material quality loss is influenced by mechanical factors.
Vacuum heat treatment of the problem
Vacuum heat treatment processing, the processing surface of the product is often a problem, "colored" areas appear. Obtain appearance of bright, no coloring effect is the common goal of product processing vacuum furnace manufacturers and users to pursue research and development.
Vacuum heat treatment technology to resolve
Comprehensive technology of vacuum heat treatment vacuum technology and heat treatment technology of two professional combination, refers to the heat treatment process of all or part of the vacuum condition. Is generally believed that the vacuum furnace is divided into high, high, medium and low vacuum.
Factors that affect the performance of the heat treatment
Today su shi heat treatment come to you of what the factors in the use of vacuum heat treatment furnace heat treatment will affect the performance of the heat treatment:

1
Brazing of aluminum frame
Product:Brazing of aluminum frame
2Cold die steel heat treatment technology
3High-frequency quenching
4Stainless solution treatment
5SUS420 blade heat treatment
6Vacuum hardening

Similar Articles

Latest News

History

  • None
Set Home Page  |Contact|News|Set Map

Su's heat treatment (Shenzhen) Co., Ltd.  Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14

(Workdays:9:30-18:00)

Online QQ



Service Hotline

0755-27291255