Welcome to SuShi Heat Treatment Ltd. Official Website!
Current location:Home>Client> S136 heat treatment

Contact SU SHI

Su's heat treatment(Shenzhen)Co., Ltd.
Service Hotline 0755-27291255
Fax0755-27293730

E-MAIL: sushirechuli@163.com
CompanyAddress: 14 BaiSha Road,Second Industrial Zone,Shenzhen manholeNewbridge


Client
S136 heat treatment

Editor:    Date:2014-04-10 11:25:50    Views:8382

S136 heat treatment:

___________ soft annealing

Under the protection state, after heated to 780 ℃ temperature in the furnace per hour the speed of 10 ℃, the cooling to 650 ℃, then put in air cooling.

2. Stress removal

After rough machining, which must be heated to 650 ℃, both temperature 2 hours later, the slow cooling to 500 ℃, and then put in air cooling.

3. Quenching

Preheat temperature: 600-600 ℃

Quenching temperature (austenitizing temperature) : 1020-1050 ℃

The commonly used temperature: 1030 ℃

℃ temperature holding time (minutes) before tempering hardness (HRC)

1020  30  56 ± 2

1050  30  57 ± 2

Heat preservation time = when the steel surface and center to achieve consistent after quenching temperature, to begin to calculate time of heat preservation in the furnace.

Quenching, must be protected to avoid decarburization and oxidation.

4. Cooling medium

Oil; Flow particle furnace or 250-550 ℃ graded quenching salt bath furnace, then cooling in the air; High-speed gas/have enough positive pressure of the gas in the vacuum furnace to mold to achieve the most appropriate features, in the mold deformation degree of acceptable conditions, cold speed the sooner the better. When in vacuum furnace heat treatment is recommended to use four or five bar pressure. Steel cooled to 50-70 ℃ (120-160 ° F) shall promptly tempering.

⒌ tempering

Tempering two times, each time after tempering, must be cooled to room temperature, minimum tempering temperature of 180 ℃ (applicable to small). Holding time at least two hours.

Note 1: the 250 ℃ tempering is recommended for the best combination of toughness, hardness and corrosion resistance.

Note 2: the austenitizing temperature should avoid to choose too high and too low tempering temperature < 250 ℃ combination, avoid the stress of the mould is too big.

Zhang shrinkage deformation and size of S136:

Quenching and tempering S136 time is long, the size of the high temperature easy to shrink, the material is not easy to shrink.

Prev: 40Cr Quench Next: None
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance corrosion and wear resistance
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance to corrosion and wear properties of a great relationship: the number and morphology of precipitates in the pure wear conditions, no corrosion, material quality loss is influenced by mechanical factors.
Vacuum heat treatment of the problem
Vacuum heat treatment processing, the processing surface of the product is often a problem, "colored" areas appear. Obtain appearance of bright, no coloring effect is the common goal of product processing vacuum furnace manufacturers and users to pursue research and development.
Vacuum heat treatment technology to resolve
Comprehensive technology of vacuum heat treatment vacuum technology and heat treatment technology of two professional combination, refers to the heat treatment process of all or part of the vacuum condition. Is generally believed that the vacuum furnace is divided into high, high, medium and low vacuum.
Factors that affect the performance of the heat treatment
Today su shi heat treatment come to you of what the factors in the use of vacuum heat treatment furnace heat treatment will affect the performance of the heat treatment:

1
Brazing of aluminum frame
Product:Brazing of aluminum frame
2Cold die steel heat treatment technology
3High-frequency quenching
4Stainless solution treatment
5SUS420 blade heat treatment
6Vacuum hardening

Similar Articles

Latest News

History

  • None
Set Home Page  |Contact|News|Set Map

Su's heat treatment (Shenzhen) Co., Ltd.  Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14

(Workdays:9:30-18:00)

Online QQ



Service Hotline

0755-27291255