17-4 stainless steel vacuum brazing

Editor:    Date:2014-09-10 11:29:40    Views:8242

Application of high vacuum brazing containing volatile element less. Solder, base metal and oxide to decomposition. If more contain solder in the volatile elements, in order to vapor pressure at the temperature under less solder solder, parent material and these elements, improve the brazing quality, local vacuum brazing technology can be used to access certain pressure of argon.

Prev: 304 stainless steel welding Next: None
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance corrosion and wear resistance
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance to corrosion and wear properties of a great relationship: the number and morphology of precipitates in the pure wear conditions, no corrosion, material quality loss is influenced by mechanical factors.
Vacuum heat treatment of the problem
Vacuum heat treatment processing, the processing surface of the product is often a problem, "colored" areas appear. Obtain appearance of bright, no coloring effect is the common goal of product processing vacuum furnace manufacturers and users to pursue research and development.
Vacuum heat treatment technology to resolve
Comprehensive technology of vacuum heat treatment vacuum technology and heat treatment technology of two professional combination, refers to the heat treatment process of all or part of the vacuum condition. Is generally believed that the vacuum furnace is divided into high, high, medium and low vacuum.
Factors that affect the performance of the heat treatment
Today su shi heat treatment come to you of what the factors in the use of vacuum heat treatment furnace heat treatment will affect the performance of the heat treatment:
Set Home Page  |Contact|News|Set Map

Su's heat treatment (Shenzhen) Co., Ltd.  Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14

(Workdays:9:30-18:00)

Online QQ



Service Hotline

0755-27291255