Cryogenic treatment is not all retained austenite transforms into martensite, even if repeated cryogenic treatment, 5%-10% still retained austenite, cryogenic treatment will be retained austenite block breaking into film. And distribution in the martensite edge, can reduce the stress concentration at the edge, is beneficial to increase the strength of steel. But between martensite stable residual austenite microstructure composite tissue membrane and dispersed Markov body in different orientation of carbide. Have strong toughness, best.
(1) LD steel after cryogenic treatment is not complete transformation of retained austenite, repeat after cryogenic treatment still has residual austenite.
(2) LD steel after quenching and cryogenic treatment, quenching and tempering, cryogenic treatment with strong toughness, strength and composite cryogenic treatment has better strength and toughness and wear resistance, repeated cryogenic treatment effect is better.
-
1
Brazing of aluminum frameProduct:Brazing of aluminum frame
Similar Articles
- Welding method of cast iron parts
- Reduce large structure welding deformation technological countermeasures
- Welding history
- Laser spot welding technology is analysed
- The way to prevent the welding spatter
- Titanium alloy laser repair welding technology
- The welding of titanium alloy and testing
- The point of use of stainless steel electrode should notice
- The role of argon gas in welding
- The impact of high temperature alloy welding
Latest News
- Welding method of cast iron parts
- Reduce large structure welding deformation technological countermeasures
- Welding history
- Laser spot welding technology is analysed
- The way to prevent the welding spatter
- Titanium alloy laser repair welding technology
- The welding of titanium alloy and testing
- The point of use of stainless steel electrode should notice
- Welding transverse crack reason mainly has the following several aspects
- The role of argon gas in welding
History
- None
Su's heat treatment (Shenzhen) Co., Ltd. Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14