Alloy elements in steels have influence on the welding
Aluminum: aluminum is used as a cleaning agent grain refinement and deoxidization. Aluminum can significantly reduce the strain aging brittleness, excess aluminum will reduce the toughness of steels.
S: for the harmful elements, which makes the plasticity and toughness of steel decreases, especially the toughness effect is more apparent, have an adverse effect on the welding.
P: harmful elements, slashing the plasticity and impact toughness, improve the brittle temperature of steel, steel welding crack susceptibility.
The above is the alloy elements in Shenzhen sushi heat treatment summary of the impact of welding, Shenzhen Su's heat treatment to undertake professional stainless steel welding, aluminum brazing, heat treatment orders.
-
1
Brazing of aluminum frameProduct:Brazing of aluminum frame
Similar Articles
- Welding method of cast iron parts
- Reduce large structure welding deformation technological countermeasures
- Welding history
- Laser spot welding technology is analysed
- The way to prevent the welding spatter
- Titanium alloy laser repair welding technology
- The welding of titanium alloy and testing
- The point of use of stainless steel electrode should notice
- The role of argon gas in welding
- The impact of high temperature alloy welding
Latest News
- Welding method of cast iron parts
- Reduce large structure welding deformation technological countermeasures
- Welding history
- Laser spot welding technology is analysed
- The way to prevent the welding spatter
- Titanium alloy laser repair welding technology
- The welding of titanium alloy and testing
- The point of use of stainless steel electrode should notice
- Welding transverse crack reason mainly has the following several aspects
- The role of argon gas in welding
History
- None
Su's heat treatment (Shenzhen) Co., Ltd. Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14