1, using fast precooling isothermal spheroidizing process, through the rapid pre cooling increase the supercooling degree, can improve the speed of the ball, the annealing time is shortened to the traditional process of 1/7~1/10.
2, heating to 860 ℃ ~940 ℃, 730 ℃ isothermal 1.0~1.5h, can get fine particles, carbide distribution, hardness nodular structure appropriate to heated to 940 ℃, the best effect.
3, the heating temperature is too high or the holding time is too long, causing most of carbide dissolution, precipitation is unfavorable for the granular carbides.
| Prev: Causes of quenching distortion and cracking of the linear cutting | Next: Effects of pulse parameters on Gas Nitrocarburizing layer depth |
-
1
Brazing of aluminum frameProduct:Brazing of aluminum frame
Similar Articles
- Welding method of cast iron parts
- Reduce large structure welding deformation technological countermeasures
- Welding history
- Laser spot welding technology is analysed
- The way to prevent the welding spatter
- Titanium alloy laser repair welding technology
- The welding of titanium alloy and testing
- The point of use of stainless steel electrode should notice
- The role of argon gas in welding
- The impact of high temperature alloy welding
Latest News
- Welding method of cast iron parts
- Reduce large structure welding deformation technological countermeasures
- Welding history
- Laser spot welding technology is analysed
- The way to prevent the welding spatter
- Titanium alloy laser repair welding technology
- The welding of titanium alloy and testing
- The point of use of stainless steel electrode should notice
- Welding transverse crack reason mainly has the following several aspects
- The role of argon gas in welding
History
- None
Su's heat treatment (Shenzhen) Co., Ltd. Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14