Heat treatment process for high quality spring steel

Editor:    Date:2014-08-12 14:53:14    Views:5369

With the rapid development of automotive lightweight and heavy railway acceleration, both automobile suspension spring or train bogie spring, is toward the direction of high strength, high stress, high quality and high reliability direction. Effectively improve the fatigue life and the spring steel anti resistance not only ensured by improving steel purity, and to strictly control the rolling and heat treatment system to increase the strength and toughness of steel. There are mainly two kinds of heat treatment process on the spring manufacturing process at present, one is to quenching technology, another is the volume of direct heat quenching process. Reheating quenching process refers to the spring steel is heated roll forming air cooling to room temperature, then re heated to a heat treatment process of austenitizing temperature quenching. The quenching process is a spring steel heating rolled into spring, using a heat treatment process of the waste heat of direct quenching. The austenitizing temperature, quenching and tempering process parameters affect the mechanical performance of the final product.

Prev: Shenzhen Su's heat treatment to achieve heat treatment process of computer management and control Next: Shenzhen Su's heat treatment of heat treatment gas sources and metallurgical problems in the standards
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance corrosion and wear resistance
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance to corrosion and wear properties of a great relationship: the number and morphology of precipitates in the pure wear conditions, no corrosion, material quality loss is influenced by mechanical factors.
Vacuum heat treatment of the problem
Vacuum heat treatment processing, the processing surface of the product is often a problem, "colored" areas appear. Obtain appearance of bright, no coloring effect is the common goal of product processing vacuum furnace manufacturers and users to pursue research and development.
Vacuum heat treatment technology to resolve
Comprehensive technology of vacuum heat treatment vacuum technology and heat treatment technology of two professional combination, refers to the heat treatment process of all or part of the vacuum condition. Is generally believed that the vacuum furnace is divided into high, high, medium and low vacuum.
Factors that affect the performance of the heat treatment
Today su shi heat treatment come to you of what the factors in the use of vacuum heat treatment furnace heat treatment will affect the performance of the heat treatment:

1
Brazing of aluminum frame
Product:Brazing of aluminum frame
2Cold die steel heat treatment technology
3High-frequency quenching
4Stainless solution treatment
5SUS420 blade heat treatment
6Vacuum hardening

Similar Articles

Latest News

History

Set Home Page  |Contact|News|Set Map

Su's heat treatment (Shenzhen) Co., Ltd.  Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14

(Workdays:9:30-18:00)

Online QQ



Service Hotline

0755-27291255