1: by adding Ni, Mo, Mn alloying elements and proper austenitizing temperature quenching to obtain good performance of the martensite / bainite dual phase grey cast iron.
2: when quenching around graphite undercooled austenite priority into lower bainite, and the internal micro stresses in the transformation of Shi Mojian lower bainite more fully.
3:reasons: due to the segregation of Mn, Mo elements, quenching early formation of a large number of stable residual austenite "white area" in the eutectic cell boundary, the hardness can reach 800HV, 250 ℃ for long time tempering can make its part into a high carbon martensite, but can not be completely eliminated.
We
| Prev: Shenzhen Su's heat treatment processing that Cr20 heat treatment process | Next: Austenite transformation sequence and organization of the nucleation characteristics |
-
1
Brazing of aluminum frameProduct:Brazing of aluminum frame
Similar Articles
- Welding method of cast iron parts
- Reduce large structure welding deformation technological countermeasures
- Welding history
- Laser spot welding technology is analysed
- The way to prevent the welding spatter
- Titanium alloy laser repair welding technology
- The welding of titanium alloy and testing
- The point of use of stainless steel electrode should notice
- The role of argon gas in welding
- The impact of high temperature alloy welding
Latest News
- Welding method of cast iron parts
- Reduce large structure welding deformation technological countermeasures
- Welding history
- Laser spot welding technology is analysed
- The way to prevent the welding spatter
- Titanium alloy laser repair welding technology
- The welding of titanium alloy and testing
- The point of use of stainless steel electrode should notice
- Welding transverse crack reason mainly has the following several aspects
- The role of argon gas in welding
History
Su's heat treatment (Shenzhen) Co., Ltd. Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14